Nickel etchant for evaporated nickel films
Thermo Scientific Chemicals

Nickel etchant for evaporated nickel films

Standard nickel etchant for evaporated nickel films
製品番号(カタログ番号) 044586.R0
または、製品番号044586-R0
価格(JPY)
-
数量:
1 qt.
一括またはカスタム形式をリクエストする
仕様
化学物質名または材質Nickel etchant for evaporated nickel films
Colorless to Yellow
DOT情報Transport Hazard Class: 8; Packing Group: III; Proper Shipping Name: CORROSIVE LIQUID, ACIDIC, INORGANIC, N.O.S.
健康被害1H290-H314-H331-H360D-H362
健康被害2GHS H Statement
H314
Causes severe skin burns and eye damage.
さらに表示
Standard nickel etchant for evaporated nickel films

This Thermo Scientific Chemicals brand product was originally part of the Alfa Aesar product portfolio. Some documentation and label information may refer to the legacy brand. The original Alfa Aesar product / item code or SKU reference has not changed as a part of the brand transition to Thermo Scientific Chemicals.

RUO – Research Use Only

よくあるご質問(FAQ)

What is the etch rate of Nickel etchant for evaporated nickel films at 30 degrees C?

Nickel etchant for evaporated nickel films has an etch rate of 25 Å/second at 30 degrees C.

How do I reduce undercutting of an etchant?

Undercutting of the etchant can be reduced by increasing the rate of stirring or agitation.

Do I need to dilute an etchant?

No, it is a ready-to-use solution. Dilution will only be necessary if you want to reduce the etch rate.

How do I reduce the etch rate of an etchant?

The etch rate of the etchant can be reduced by adding 1 part deionized water to 2 parts etchant. This will reduce the etch rate approximately 50%.

How do I increase the etch rate of an etchant?

The etch rate of the etchant will be increased by increasing the rate of stirring or agitation.